Clay Firing process

After all of the drying process are finished, we start to put the molded clay in a firing place. The firing process can be started when the stuffs is still warm to avoid from breakage to get sudden heat. This process is usually takes about 10 to 12 hours with about 900 to 1100 degrees in Celsius. After the firing process is finished, we do need to wait at least 12 hours before the stuff can be unloaded from firing place to get the temperature is going down.